Design and Reliability of Ceramics: Do Modelers, Designers, and Fractographers see the same world?

Published

Author(s)

George D. Quinn
Proceedings Title
Conference on Advanced Ceramics and Composites
Conference Location
Cocoa Beach FL,
Conference Title
Ceram. Eng. and Sci. Proc., Volume: 26(8) pages 239-252

Citation

Quinn, G. (2005), Design and Reliability of Ceramics: Do Modelers, Designers, and Fractographers see the same world?, Conference on Advanced Ceramics and Composites , Cocoa Beach FL, , [online], https://tsapps.nist.gov/publication/get_pdf.cfm?pub_id=854270 (Accessed May 10, 2025)