Vaish, A.
, Krueger, S.
, Dimitriou, M.
, Majkrzak, C.
, Vanderah, D.
, Chen, L.
and Gawrisch, K.
(2014),
Enhancing the Platinum Atomic Layer Deposition Infiltration Depth inside Anodic Alumina Nanoporous Membrane, Journal of Vacuum Science & Technology A, [online], https://tsapps.nist.gov/publication/get_pdf.cfm?pub_id=916571