NIST Recommended Practice Guide: Fractography of Ceramics and Glasses, 3rd edition

Published

Author(s)

George D. Quinn

Abstract

Fractography is a powerful but underutilized tool for the analysis of fractured glasses and ceramics, for fractures in the laboratory and for component failures in service. Fractography can identify the cause of failure and can even provide quantitative information about the loading conditions. The goal of this Guide from the beginning has been to make fractographic analysis of brittle materials less an art and more an engineering practice for scientists and engineers. This Guide is a free public service of NIST for the benefit of American industry, and the worldwide ceramic and glass communities. This 3rd edition in 2020 adds some new developments in our field, new equipment and techniques, and some new case studies. The fundamentals of fractography of ceramics and glasses are unchanged. The revisions are refinements, clarifications, and addition of new examples. It expands some topics glossed over (e.g., terminal crack velocities) in the earlier editions.
Citation
Special Publication (NIST SP) - 960-16 3rd ed
Report Number
960-16 3rd ed

Keywords

fractography, glasses, ceramics, fracture origin, fracture mechanics, microscopy, Dentistry

Citation

Quinn, G. (2020), NIST Recommended Practice Guide: Fractography of Ceramics and Glasses, 3rd edition, Special Publication (NIST SP), National Institute of Standards and Technology, Gaithersburg, MD, [online], https://doi.org/10.6028/NIST.SP.960-16e3 (Accessed May 9, 2025)

Issues

If you have any questions about this publication or are having problems accessing it, please contact [email protected].

Created September 14, 2020, Updated July 22, 2024