Szczepanowska, H.
and Renegar, T.
(2014),
Surface Analysis and Materials Characterization for the Study of the Ceramic Tiles HRSI from the Space Shuttle Thermal Protective Systems, Journal of Materials Science & Technology, [online], https://tsapps.nist.gov/publication/get_pdf.cfm?pub_id=916428